1. Probable Cause / Reason:
• Exposure of the curing paint film to moisture or condensation.
• Application and curing at low temperatures, affecting amine-cured epoxies.
• Incorrect or imbalanced solvent blend during paint formulation or application.
• Humid or poorly ventilated conditions during the curing process.
2. Correction / Repair:
• Wash the affected surface with clean water and mild detergent to remove blush.
• Lightly abrade the surface if necessary to restore proper adhesion.
• Reapply topcoat or finish coat under correct environmental conditions.
• Ensure full removal of contaminants before recoating to prevent recurrence.
3. Corrective Action / Prevention:
• Apply and cure coatings in recommended temperature and humidity ranges.
• Use correct solvent blends and follow manufacturer's application guidelines.
• Ensure good ventilation and dry conditions during and after application.
BG GROUP OF PAINT AND COATING CONSULTANT
Email: support@bgcoating.com / inquiry.bggroup@gmail.com
Website: https://bgcoating.com
LinkedIn: https://www.linkedin.com/company/bggroupofpaintandcoatingconsultant/
Google My Business: https://maps.app.goo.gl/pUMmXu4D5tPhpnbh9
Booking Appointment: https://forms.gle/YaYPVNUT6ai3Ucuj9