1. Probable Cause / Reason:
• Insufficient film thickness of the topcoat, leading to poor coverage.
• Poor opacity and covering power of the topcoat.
• Strong color or contrast from the primer or undercoats showing through.
• Applying lighter colors over dark-colored primers or undercoats.
2. Correction:
• Apply adequate dry-film thickness between individual coats to ensure full coverage.
• Use coatings with good opacity and hiding power to cover the underlying surface effectively.
• Apply additional coats if necessary to achieve full coverage and prevent the underlying surface from showing through.
• Consider using a primer or undercoat with better hiding properties.
3. Corrective Action / Prevention :
• Remove the affected coating and ensure proper surface preparation before re-coating.
• Reapply the topcoat with sufficient thickness to hide the underlying surface.
• Use coatings with higher opacity or better hiding power for future applications.
BG GROUP OF PAINT AND COATING CONSULTANT
Email: support@bgcoating.com / inquiry.bggroup@gmail.com
Website: https://bgcoating.com
LinkedIn: https://www.linkedin.com/company/bggroupofpaintandcoatingconsultant/
Google My Business: https://maps.app.goo.gl/pUMmXu4D5tPhpnbh9
Booking Appointment: https://forms.gle/YaYPVNUT6ai3Ucuj9