1. Probable Cause / Reason:
• Trapped air or solvent inside the coating, not escaping before drying.
• Air entrainment during mixing of the coating material.
• High ambient temperature during application affecting drying behavior.
• Overcoating without properly cleaning surfaces like antifouling or zinc silicates.
2. Correction / Repair:
• Sand down the affected area to remove bubbles or craters.
• Properly clean and prepare the surface before recoating.
• Adjust spray parameters, including viscosity and application temperature.
• Reapply coatings with correct techniques, ensuring thin and even layers.
3. Corrective Action / Prevention:
• Use correct mixing methods and equipment to avoid air entrapment.
• Apply a mist coat initially and use defoaming agents when necessary.
• Follow product data sheets strictly for temperature and application conditions.
BG GROUP OF PAINT AND COATING CONSULTANT
Email: support@bgcoating.com / inquiry.bggroup@gmail.com
Website: https://bgcoating.com
LinkedIn: https://www.linkedin.com/company/bggroupofpaintandcoatingconsultant/
Google My Business: https://maps.app.goo.gl/pUMmXu4D5tPhpnbh9
Booking Appointment: https://forms.gle/YaYPVNUT6ai3Ucuj9