1. Probable Cause / Reason:
• Poor flow and leveling of the paint film
• Incorrect spray technique or gun settings
• Wrong solvent blend or fast evaporation rate
• High thixotropy (paint too thick or not properly mixed)
2. Correction:
• Sand the affected area to smooth out the surface
• Clean thoroughly and ensure surface is dust-free
• Adjust spray parameters and solvent selection
• Recoat with correct technique and material mix
3. Corrective Action / Prevention:
• Use recommended spray settings and equipment
• Ensure proper thinning and mixing of paint
• Apply in suitable environmental conditions for flow-out